Follow Us: iconfinder 5365678 fb facebook facebook logo icon 64px   iconfinder 5296765 camera instagram instagram logo icon 64px   iconfinder 5296516 tweet twitter twitter logo icon 64px   youtube 64px

The same process was employed for the canopy, but a stronger water stain was used due to the soft open grain and very light orange colour of the cedar wood. Once stained it was sealed with 50/50% shellac and meths but then had two polish rubber coats of shellac to fill the grain.
 
 
  CBC26
  Stained, polished and ready for waxing.
 
Once all three sections were finished with a shellac polish, they were waxed with pigmented beeswax and left overnight to harden. Then they were brushed off and burnish-polished to finish.  
 
  CBC27
 
Once reassembled, the bed has had no further treatment.